Qinghe.
EN
Home / Blog / Construction / 24 Nov 2026

Chrome, Powder or Plating: What Each One Costs You in Service

Three finishes that look like metal, three very different repair stories. One of them cannot be touched up at all.

Part of the construction guide — How a Contract Chair Is Built

Powder coat

Sprayed and cured, 60–80 micron, cured at 180–200 °C. Thick enough to hide small surface variation and available in any RAL. Damage is local and repairable with a touch-up pen or a small spray can.

Weakness: it is a plastic film. One chip at a corner exposes steel and the chip grows as rust lifts the film from beneath. On a chair leg that gets kicked, a chip is a two-year countdown.

Chrome plating

Electroplated over polished steel or brass. Hard, thin and mirror-bright. The layer is measured in microns and any breakthrough is a corrosion site that cannot be hidden.

Weakness: it cannot be repaired in the field. The scratch stays a scratch, and re-plating a chair frame means stripping and re-polishing the whole frame, which costs more than a new frame.

Brushed or satin metal finishes

Mechanically finished stainless or plated then brushed. Hides fingerprints, reads warm, and small scratches blend into the grain direction. The most forgiving of the three in service.

Weakness: cost. Stainless in furniture sections is two to three times powder coat, and it needs a different welding process to keep the corrosion resistance at the weld.

Choosing by room

Kitchen-adjacent and back-of-house: powder coat, because it takes knocks and hides them. Front of house with a design intent for metal: brushed. Chrome only where nothing will ever touch it, which in a dining room is nowhere.

Coating prep decides whether any of the three survives a cleaning regime, covered in powder coat prep. Steel section sizes sit in steel tube wall thickness.

Where this applies

More from the workshop

Have a room to fit out?

Send the floor plan and the seat count. Quote and finish chip in one reply.

Start a conversation →