So this guide works through the frame joint by joint, with the loads and the details that hold them. Every note on this site about frames comes back to these four points.
Contract seating is tested at EN 16139 level 2 (contract) — static load 1,600 N on the seat, 560 N on the back. Put plainly: sit down hard, then lean back with your weight on the backrest. The seat takes roughly three times the load of the back, but the back is where the frame flexes, so the joint at the top of the leg does more work than its share of the number suggests.
The chair also gets dragged, tipped onto two legs and used as a step. None of that is in the standard and all of it happens in a buffet hall at eight in the morning.
Mortise and tenon. 10–12 mm mortise, 25–35 mm deep, glued and pinned. The strongest option for a timber frame and the one that takes the back load best. Costs more because it is slower to machine.
Dowel joint. three 8 mm or 10 mm beech dowels per corner, 30 mm into each part. Common on mid-price frames. Three dowels per corner is fine for a side chair in a guest room; two is where it starts to rack.
Corner block. glued and screwed block behind the leg and rail, hidden under the seat. This is the detail that decides whether a dowel frame survives. Corner blocks are cheap and it is the first thing to disappear from a cheap quotation.
MIG weld. 1.2–1.5 mm wall tube, 360° fillet, ground before powder. On steel frames the weld replaces all three of the above, and the quality question moves to penetration and post-weld cleanup.
16–25 mm diameter round, or 25 × 25 mm square tube at 1.2–1.5 mm wall. Thinner than 1.2 mm and the tube dents at the leg where it meets the floor; thicker than 1.5 mm and the chair is heavier than the job needs.
Pretreatment is four-stage: degrease, rinse, conversion coating, dry. Skip a stage, usually the conversion coating, and the powder adheres to a surface that is not bonded to the steel. It looks fine and lifts in sheets after two years of cleaning chemicals.
Powder at 60–80 micron, cured at 180–200 °C, tested at 500 hours neutral salt spray on a test coupon per batch. Ask for the coupon, not the certificate — a coupon is a physical part from the actual batch.
12 mm birch plywood, stapled, or elastic webbing at 50 mm centres. 35–45 kg/m³ for seat pads, 25–30 kg/m³ for backs, 40–50 mm seat, 20–30 mm back. Below 35 kg/m³ foam the seat bottoms out under a 90 kg guest within a year, and the cover then takes the wear the foam should have absorbed.
Moulded foam at 45–55 kg/m³ moulded foam is what a shaped seat needs. Cut foam on a flat pan gives the same comfort everywhere, which is why cheap chairs feel fine in the showroom and hard after an hour.
Front leg joint at the seat rail. Back post at the height of the seat. Corner block glue line. Then the seat foam, then the cover, then the finish. The frame outlives the upholstery by years, which is why the re-cover question belongs in the specification.
If a chair comes back broken in the first year, the failure is almost always in the first two items on that list, and both of them are hidden under the seat when the chair is standing normally.
Send it over. We will mark the joints, the species by part and the sizes that need confirming.
Send the drawing →