Rust starts in the seam beside a weld, not on the weld. Two sharp edges, a gap of 0.2 mm and no way for the pretreatment to reach inside.
Where a tube meets a plate, the weld leaves a crevice along its toe. Pretreatment chemicals cannot flush it, powder cannot reach into it, and water sits in it. That geometry is a corrosion cell by definition.
Salt spray testing on a flat coupon passes at 500 hours neutral salt spray on a test coupon per batch. The same coating on a welded seam fails in a fraction of that, because the test coupon had no crevice.
Continuous weld. Weld the full perimeter instead of stitching. Slower and it adds distortion, but it removes the crevice.
Seam sealant. Capillary sealant applied after pretreatment and before powder, drawn into the gap. Common in automotive, rare in furniture, and it works.
Design the joint open. Leave a 2 mm gap so pretreatment and powder both reach the surfaces, and there is no capillary to hold water. Counter-intuitive and often the cheapest fix.
The bottom of the leg where it meets the foot plate, and the seat frame where the leg tube is welded on. Both are at floor level, both take mop water, and both are the first place a guest notices rust on a chair.
On a hotel with daily mopping, an untreated seam shows orange staining within eighteen months. That staining then marks the floor, and the floor is more expensive than the chair.
Continuous weld or open joint at floor-level connections, seam sealant on the rest, and a salt-spray test on a production frame rather than a flat coupon. Test the frame, not the panel.
Rust at the weld toe is different from a weld that has failed, which is covered in weld quality on a chair frame. Pretreatment detail sits in powder coat prep.