RAL 7016 on one order and RAL 7016 on the next are not the same grey. The powder is the same code and the film is a different thickness.
Film thickness changes colour. Sixty microns over a light grey primer reads lighter than an 80 micron coat of the same powder. 60–80 micron, cured at 180–200 °c. That spread is enough to see on a large flat panel and just enough to argue about on a chair.
Substrate matters too. The same powder over blasted steel and over a conversion coating cures to slightly different gloss, because the surface under it reflects differently.
Powder comes in batches with a lot number. Two lots of RAL 7016 from the same supplier can differ by two Delta-E units, which is the threshold where the eye starts to notice side by side.
Record the lot number per order and keep a sprayed coupon from each lot. On a repeat order, send the coupon — a supplier can match a physical sample, and cannot match a code alone.
Rows of chairs in the same light. Not stacks, not single chairs. Twenty frames side by side make a half-unit difference obvious, and that is how a hotel inspector sees the room.
Gloss is the second variable. 30% gloss and 70% gloss in the same RAL read as two colours under downlights, and neither is wrong against the code.
Code, gloss level, film thickness range and the lot number. Four items. Add "one retained coupon per lot" and the next order can be matched instead of guessed.
Prep and curing decide whether the colour survives a cleaning chemical, which is covered in powder coat prep. Salt spray figures sit in the construction guide.
Send the floor plan and the seat count. Quote and finish chip in one reply.