The same 25 mm top with a banded edge and a lipped edge looks identical on a sample. They part company in month eighteen, at the edge a cloth gets wrung out over.
The core is the vulnerable part. Fibreboard at 720 kg/m³ takes water through an exposed edge faster than through any face, and a 25 mm panel that absorbs water swells about 8 per cent in thickness, which is 2 mm of bump along one edge. On a dining table, 2 mm is enough to catch a cloth and to lift the top off a level check.
Band thickness is all that stands between the core and a wipe-down. 3 mm ABS covers the joint line and takes the first knocks. 0.5 mm melamine edge is a decorative line and does nothing structural.
The band rarely wears through. It lifts. Warm water sits in the 0.2 mm gap between band and face, the adhesive softens around 60 °C, and a housekeeping cloth pulls the edge back a millimetre at a time. Once water reaches the core, the swell pushes the band off from behind and no glue holds it again.
Two details slow that down: a 1 mm chamfer on the top edge so the cloth rides over the joint instead of catching it, and a band applied after the face is sealed rather than before. Neither costs anything on a new order and both are usually missing.
Solid lipping of 25 to 30 mm, glued to the core and machined flush with the face, moves the wear line off the joint entirely. The edge becomes end grain of the same species as the face, so a sanding and a coat of the same sealer brings it back. Two re-finishes over ten years are realistic on a lipped top, and zero on a banded one.
Price is per metre of perimeter, and a 1,200 × 800 mm top carries 4 m of it. Banded edge runs at roughly a third of the lipped price per metre. On 200 tables that gap is a line item someone will question, and the answer is how many wipe-downs that edge sees in a week.
The 3 mm radius concentrates a chair-back knock on a 3 mm line. 6 mm spreads it over twice the area and, on a lipped top, leaves material for a second sanding. Round tops under 900 mm are usually banded because the curve makes lipping expensive to run. Rectangular tops in a buffet hall are usually lipped.
The test worth writing into the order is crude and takes a day: stand the top on edge in 10 mm of water for 24 hours, then try a 0.1 mm feeler at the joint. Anything the feeler enters has failed already. Top sag over the same span is covered in apron depth and top sag.
Four notes settle the edge: core material and density, band or lipping thickness in millimetres, edge radius, and a finish line for the edge written separately from the face. Without the last one the edge gets a single coat while the face gets three, and the joint opens at the first winter.
Base spread and the tip test belong to the same drawing and are covered in table base spread and tip test. Frame and joint details across the range are in the construction guide, and the models available with a lipped top are listed under hotel dining tables.
Send the floor plan and the seat count. Quote and finish chip in one reply.
Start a conversation →