The screw is not the problem. Where it goes and how the load reaches it is. Three fixes, in order of cost.
The screw driven into the end grain of a rail holds about a third of what it holds across the grain, because the thread has nothing to bite. Pull a chair sideways and that screw is being asked to resist a lever it cannot resist.
Any fixing into an end needs a different device: a dowel, a cross dowel with a bolt, or a plate. Screws belong in face grain, and only where the load is compression or shear along the part.
The seat carries 90 kg down. That load reaches the legs through the rails, and the rails are loaded in bending. The rail fixed at both ends with two screws takes the bending at the joint, which is exactly where the section is weakest.
Better: let the rail bear on a shoulder. The tenon with a shoulder transfers load through timber contact, and the pin only stops the joint pulling apart. Screws alone carry everything through their shank, which is a 4 mm steel wire holding a chair together.
Corner block. glued and screwed block behind the leg and rail, hidden under the seat. Cheap, invisible and effective — it gives the rail a second load path.
Through-bolt with cross dowel. Used on knock-down tables and booth frames. Used where a joint must come apart again.
Glued tenon with two pins. 10–12 mm mortise, 25–35 mm deep, glued and pinned. The strongest of the three and the one that costs the most machining time.
When a screw has stripped out on site, do not go up a gauge — that splits the rail. Drill out to 8 mm, glue in a beech dowel, cut flush and re-drive the same screw into fresh timber. It takes five minutes and holds better than the original fixing.
On more than a handful of chairs, the joint pattern is wrong and the fix is a new batch of rails. Joint options are set out in mortise and tenon versus dowel, and the block detail in corner blocks and racking.
Send the floor plan and the seat count. Quote and finish chip in one reply.