Cutting, bending, welding, grinding, coating. Five stages and one of them decides whether the frame is straight.

Part of the factory guide — Inside a Chair Workshop in Lecong

The stages

Tube cut to length, bent on a mandrel, welded in a jig, ground at the weld, then coated. 1.2–1.5 mm wall tube in 16–25 mm diameter round, or 25 × 25 mm square.

Bending is where most shops lose accuracy. The mandrel bender holds the section; a press bender flattens it slightly and the frame is never quite square.

Welding quality

1.2–1.5 mm wall tube, 360° fillet, ground before powder. The 4 mm fillet on 1.5 mm wall burns through; a 2.5 mm fillet is correct.

Ground welds look better and lose a little strength at the toe. Unground welds are honest and show whether the operator can run a consistent bead.

Coating line

Four-stage: degrease, rinse, conversion coating, dry. Then powder at 60–80 micron, cured at 180–200 °C, and a salt spray check at 500 hours neutral salt spray on a test coupon per batch.

The shop without pretreatment is a shop where powder fails at the seams within two years.

What to check

Set two frames side by side on a flat table and measure the diagonal difference. Then look at a weld under the seat where nobody sees it — that is the weld that shows the real standard.

Weld detail sits in weld quality on a chair frame, and coating in powder coat prep.