Qinghe.
EN
Home / Blog / Factory / 24 Nov 2026

Inside a Spray Booth: What Decides a Finish

Same lacquer, same colour, two different results. The variables are air, temperature, film thickness and time.

Part of the factory guide — Inside a Chair Workshop in Lecong

The four variables

Airflow and filtration, booth temperature, film thickness per coat, and flash-off time between coats. Change any one and the finish changes.

Which is why a finish approved in June can arrive slightly different in December — the booth was colder and the coats went on thicker.

Film thickness

Measured in microns on a cured part. The 30 micron coat and a 60 micron coat of the same lacquer read as two colours on a large panel.

Two thin coats beat one thick coat for durability and for evenness. One thick coat sags, cures unevenly and yellows faster.

Curing

Forced drying at 40–50 °C for a set time, then cooling before stacking. Stacking warm parts marks them and traps solvent.

Solvent trapped under a coat blushes white in a humid month — the defect appears weeks after delivery.

What to check on a delivery

Look along a flat panel in raking light for sags and nibs. Then check the edges, where the film is thinnest and wear starts.

Colour under daylight, not under the factory's lamps. Finishing records sit in the factory guide, and colour matching in powder coat colour matching.

Where this applies

More from the workshop

Have a room to fit out?

Send the floor plan and the seat count. Quote and finish chip in one reply.