Two ways to make a curve, two different products. The sample tells you which one you bought, and the price usually tells you first.
Solid blanks go into a steam box at about 100 °C for roughly an hour per 25 mm of thickness. Hot lignin softens, the blank goes into a jig within seconds, and it stays there until it cools. Come out, spring back, settle.
It only works on species that cooperate. Best of the group; the classic bent-back timber; excellent. Try it on Acacia and the blank tears on the outside of the curve.
Thin veneers — 3 to 5 mm — glued in a former under pressure. No steam, no lignin, no springback to speak of, because each layer is thin enough to conform. The result is stronger than a steam-bent part of the same section, because glue lines replace the natural weak point.
It also uses a fraction of the timber, since offcuts and short stock work fine as veneer. That is why a laminated back can cost half of a steam-bent one at the same radius.
Because a laminate looks like a laminate. Five glue lines along a curved back are visible on the end grain and along the edge, and on a chair where the back is the design, that is the part the client will look at.
And because a bad laminate fails differently. Steam bending fails by tearing on the outside of the curve, which the workshop sees immediately. Laminating fails by delaminating, which happens six months later on a chair in service, and usually on the batch that was pressed on a Friday.
Say which one you want. "Solid ash, steam bent, one piece, no lamination" is a specification. Curved back, ash" is not, and the supplier is free to laminate it and charge for the steam bend.
On the sample, look at the end grain at the top of the back. Steam-bent solid shows continuous grain with a growth-ring pattern that follows the curve. Laminated shows parallel lines across the section. Then look at the inside face for the press marks — a laminate pressed on a rough former carries faint facets.
Either is a legitimate product. Paying steam-bend money for a laminate is not. Radius limits by species are in the chair timber guide, and the joint side of the same frame is covered in grain direction in a back post.
Send the floor plan and the seat count. Quote and finish chip in one reply.
Start a conversation →