Qinghe.
EN
Home / Guides / Timber

Chair Timber: What Actually Holds a Guest Up

Think of a dining chair as a lever with a person on the end of it. Sit down hard and the back posts take the load first, then the seat rails, then the joints where the two meet. The timber has to survive that cycle a hundred times a day for ten years, which is a different job from looking good in a photograph.

So the question is never which wood is best. It is which wood is right for the part it is asked to be. Back posts, bent backs, aprons and table tops want three different things from the same log.

The eight species we actually work with

This is the table we use in the sample room. Hardness is Janka, which is the force needed to push a steel ball halfway into the face grain — a high number means the surface resists dents, not that the joint holds better. Density is at 8–10% moisture.

SpeciesDensityJanka (lbf) BendingWhere it belongs on a chairWhere it fails
European beech
Fagus sylvatica
700–750 kg/m³1,300excellent; takes steam bending and tight radiichair frames, legs, back posts, bent backswet rooms unless sealed; moves if the kiln overshoots
Ash
Fraxinus excelsior
650–700 kg/m³1,320best of the group; the classic bent-back timberbent backs, arm bows, spindle backswide flat panels — it moves more than its density suggests
White oak
Quercus alba
750–770 kg/m³1,360good, but springs back more than beechlegs, aprons, table tops, exposed framesthin bent parts; ring-porous grain splits along the earlywood
Rubberwood
Hevea brasiliensis
600–650 kg/m³1,000poor; will not take a tight bend without laminatingbudget frames, internal rails, painted bodiesanything that carries a lever force; untreated rubberwood is borer food
Acacia
Acacia mangium / hybrid
700–750 kg/m³1,700poortable tops, seat slabs, outdoor-adjacent piecesthin legs and bent parts
Black walnut
Juglans nigra
640–660 kg/m³1,010fairvisible aprons, feature backs, top-end guest roomshigh-wear arms and legs where hardness matters
Teak
Tectona grandis
620–660 kg/m³1,050fairterrace and poolside seating, anything that sees raininterior work where the price is not justified
Poplar
Liriodendron / Populus
400–450 kg/m³540fairpainted internal frames, drawer boxes, jig workany exposed structural part

The two columns on the right are the ones buyers skip and then pay for. Acacia is the hardest timber on the list at 1,700 lbf and it is still a poor choice for a leg, because the grain interlocks and a 30 mm leg turns into a split. Black walnut at 1,010 lbf is softer than most people assume and it is chosen for colour, not for wear.

Legs, back posts, bent backs, aprons: four different jobs

Legs take compression and the sideways kick of someone dragging the chair back. Straight grain, no knots within 150 mm of the joint, and a species that holds a 10 mm mortise without splitting. European beech and White oak both do this. So does Rubberwood, until the borer treatment is skipped.

Back posts are the hardest part to get right. The grain has to run continuously from the leg through the back, or the post is two pieces joined where the highest bending moment is. If the drawing shows a continuous post, the timber has to be long enough and straight enough to cut it in one piece. Short offcuts forced into a spliced post is the single most common structural shortcut in this category.

Bent backs are a bending question, not a hardness question. Ash takes steam bending better than anything else here; European beech will take a gentle curve and fight anything tighter than about a 300 mm radius. Black walnut and poor — the wrong tool for the job.

Aprons and seat rails carry the seat load across the frame. They can be a lesser species than the legs, and usually are: Poplar or a multilayer board (e0 glue) rail on a painted chair is normal and honest.

Moisture content kills more frames than species ever will

Target at packing is 8–10% at packing. The reason is the container, not the workshop. a container crossing the tropics can push 8% timber to 13% and back; starting at 8–10% leaves room for the round trip.

What goes wrong when it starts at 12%: the mortise shrinks away from the tenon on the voyage, the glue line opens, and by the time the chairs reach the property the joint is held by the pin alone. Nothing visible on arrival. Six months of service later the back post rocks, and the complaint is about "quality" rather than about a kiln schedule.

How we check it: pin meter on 20% of the batch, cut test on one piece per kiln charge. Pin meters on finished chairs tell you very little, because the reading depends on where you push it. Ask for the kiln record, not the reading.

What the specification usually gets wrong

Three patterns come up again and again on drawings.

Oak everywhere. Designers write "solid oak" across the whole chair because the client liked a floor. Oak at 750–770 kg/m³ weighs a hotel chair down, costs more than beech, and moves unevenly around the ray fleck. Where it earns its place is exposed aprons, legs and tops — not bent parts.

Teak for an indoor room. for a hotel dining room it is usually the wrong spend; the room is indoors and the budget is better in the frame joint

Walnut for the frame. walnut is a colour decision more than a structural one; at 1,010 lbf it is softer than rubberwood's reputation suggests If the budget reaches walnut, the better spend is walnut on the visible apron and beech where nobody looks.

How to check a sample in ten minutes

Weigh it. European beech side chairs land around 5.5–6.5 kg; if the sample sits at 4 kg the frame is thinner than the drawing says.

Look at the end grain on the underside of the seat rail. Continuous grain running from leg into back post shows as one unbroken figure around the corner. Spliced posts show a glue line, and a glue line at that height is a repair waiting to happen.

Push a thumb into the seat pad edge. Foam for a contract seat is seat pads, 25–30 kg/m³ and should resist; foam that bottoms out immediately is domestic grade.

Then ask for the moisture record and the species on the invoice. "Solid wood" is not a species. If two suppliers quote the same drawing at 40% apart, one of them has changed the timber, and it is almost always the species behind the upholstery.

Notes in this guide

24 Nov 2026·Timber
Beech or Ash for a Bent Chair Back
Both timbers take a curve. Only one takes the curve on your drawing. Here is how to tell which one you have been quoted for.
24 Nov 2026·Timber
Oak in a Hotel Dining Room: Where It Earns Its Price
Oak is the most requested timber and the most over-specified. Four places it pays for itself, and three where it is just a heavier invoice.
24 Nov 2026·Timber
Moisture Content at Packing: The Number Nobody Asks For
A chair leaves the workshop at 12% moisture and arrives at 9%. In between, the joints have moved. This is the cheapest thing on the specification to fix.
24 Nov 2026·Timber
Rubberwood and the Borer Question
Cheap, stable, machines fast, and turns into dust in a container if the treatment is skipped. Rubberwood is fine. Skipping the dip is not.
24 Nov 2026·Timber
Reading End Grain on a Chair Frame
Ten minutes with the chair upside down tells you more about the frame than the spec sheet does. Start at the end grain and work back.
24 Nov 2026·Timber
Solid Wood or Multilayer Board: Choosing Per Part
Nobody builds a whole booth from solid timber, and nobody builds a chair leg from board. The decision is per part, and it is a movement decision.
24 Nov 2026·Timber
What a Kiln Schedule Does to a Chair Leg
Drying is the slowest step in the workshop and the first one cut when a date gets tight. Here is what the schedule actually does, and what it costs to shorten it.
24 Nov 2026·Timber
Walnut Costs the Most and Dents the Easiest
At 1,010 lbf it is softer than rubberwood's reputation. Buy walnut for the colour and put it where hands land, not where trays land.
24 Nov 2026·Timber
Spliced Posts and Short Offcuts
A back post cut in two and glued back together looks fine on the loading bay. It fails at the height where the guest leans back.
24 Nov 2026·Timber
Acacia: Hardest on the List, Wrong for Legs
1,700 lbf and cheaper than beech per kilo. It still should not go anywhere near a turned leg, and the reason is the grain, not the hardness.
24 Nov 2026·Timber
Teak Belongs Outside
Every property that specifies teak for an indoor dining room is paying for a property the room does not need.
24 Nov 2026·Timber
Grain Direction in a Back Post
Runout is the quietest defect in a chair. Nothing looks wrong until the post snaps at the height of the seat rail.
24 Nov 2026·Timber
Grading Timber for Chair Parts
Furniture grade is a board grade. Chair parts need a part grade, and the difference is roughly a third of the waste.
24 Nov 2026·Timber
Steam Bending or Laminating a Curved Back
Two ways to make a curve, two different products. The sample tells you which one you bought, and the price usually tells you first.
24 Nov 2026·Timber
Timber Certification: What FSC Actually Covers
A certificate on the invoice is not a certificate on the chair. Here is what the custody paper does and does not prove.
24 Nov 2026·Timber
The Cutting List Decides the Price
Two workshops quote the same drawing 25% apart. The difference is usually on the cutting list, not on the margin.
24 Nov 2026·Timber
Ash or Rubberwood: What the Price Difference Actually Buys
Two chairs, same shape, one quote 35% higher. The gap is not profit. It sits in three places you can check on the sample.
24 Nov 2026·Timber
Why Beech Frames Crack in the First Winter
The crack appears in January and the cause was set in August. Timber that leaves at 11% and lands in a heated room at 22% has to shrink somewhere.
24 Nov 2026·Timber
Matching a Second Order to the First, Colour and All
Hundred and eighty chairs in March, forty more in September. The forty will not match unless somebody kept the right records in March.
24 Nov 2026·Timber
Stained Beech That Reads as Oak, and Where It Stops Working
Staining beech to an oak tone saves 20% and fools most guests. It stops working at three specific points.
24 Nov 2026·Timber
The Seat Pan Is Where a Cheap Chair Fails First
The frame is still tight, the cover is still good, and the chair sags. That is a 12 mm plywood decision made two years earlier.
24 Nov 2026·Timber
MDF Curved Backs: Where They Beat Solid Timber and Where They Fail
A curved back in MDF holds its shape better than solid timber and costs a third less. It also has two failure modes that solid timber does not have.
24 Nov 2026·Timber
Knots, Sapwood and the Limits Worth Writing Into a Spec
Every timber order has knots. The argument is never about whether they exist, it is about which ones are allowed where — and that has to be on paper.
24 Nov 2026·Timber
Measuring Moisture Content When the Container Lands
A pin meter, ten minutes and a notebook settle most timber arguments before they start. The number to compare against is on the packing list.
24 Nov 2026·Timber
Joints That Open in Dry Air, and the Construction That Prevents It
High-altitude hotels, desert resorts, buildings with heat recovery and no humidification. Frames that are tight in Foshan click in the room by March.
24 Nov 2026·Timber
Timber Choice for a Hotel Dining Table Top
Tops take more abuse per square metre than any other part of the room. Four species, four honest price points, one rule about thickness.
24 Nov 2026·Timber
Reclaimed Timber in a Hotel: The Story and the Risks
Old timber has a look you cannot stain into new stock. It also arrives with nails, unknown moisture and a history of its own.
24 Nov 2026·Timber
Formaldehyde, Board Grade and What a Hotel Project Will Ask For
No guest has ever asked about the board inside a banquette base. Every hotel project asks for the certificate anyway.
24 Nov 2026·Timber
What a Container Does to Timber Between Foshan and the Hotel
Thirty-five days at sea, four climate zones, one steel box. Timber packed at 9% does not arrive at 9%.
24 Nov 2026·Timber
Timber Weight Is a Freight Line, Not a Detail
A species change that saves 8% on the frame can add 12% to the freight. On a 40HQ the two numbers are close enough to cancel out.
24 Nov 2026·Timber
Why a Timber Top Warps, and Which Warp You Can Live With
A top that has bowed 6 mm across 800 mm is not a manufacturing defect. It is a moisture gradient, and it started before the top was glued.
24 Nov 2026·Timber
Cane and Rattan Seats: Cheap to Buy, Expensive to Keep
A cane seat costs a third of an upholstered one. It also has a service life measured in months in a buffet hall, and that is the part brochures leave out.
24 Nov 2026·Timber
Open Pore or Sealed: The Finish Decision That Decides Maintenance
Both look like timber. One needs re-oiling every year, the other needs nothing until the lacquer wears through — and each one fails differently.
24 Nov 2026·Timber
Finish Aging: What Your Sample Will Look Like in Two Years
Every finish changes. The chip approved in June is not the colour delivered in June two years later, and knowing the direction of the drift is the whole trick.
24 Nov 2026·Timber
Reading a Drawing That Names Four Species
Most chair drawings do not name one timber. They name four, by part, and the buyer who misses that reads the quotation as an overcharge.
24 Nov 2026·Timber
Quarter Sawn or Flat Sawn: Paying for Stability
Same species, same log, 25% more money. Quarter sawn timber moves half as much and shows a different face — worth it on some parts and nowhere else.
24 Nov 2026·Timber
Storing Chairs on Site Without Wrecking Them
Two weeks in a humid plant room undoes a month of careful packing. The storage plan belongs in the contract, next to the delivery date.
24 Nov 2026·Timber
Fast Growth Plantation Timber: What It Changes in a Chair
Rubberwood, acacia hybrid, eucalyptus. Ten to fifteen years to harvest instead of eighty, and a frame that behaves differently for reasons you can measure.
24 Nov 2026·Timber
How Heavy Should a Dining Chair Be
There is a weight band where a chair reads as solid and still gets moved without being dragged. It is narrower than most specifications assume.
24 Nov 2026·Timber
New Chairs That Creak: Finding the Source in Ten Minutes
A creak is movement you can hear. It is never the glue — glue either holds or lets go, it does not squeak. Here is the order to check.

Drawing to check?

Send it over. We will mark the joints, the species by part and the sizes that need confirming.

Send the drawing →