Thirty-five days at sea, four climate zones, one steel box. Timber packed at 9% does not arrive at 9%.
The container loaded in a Foshan summer starts hot and humid. Crossing the tropics it can sit at 38 °C with condensing humidity on the ceiling. Rounding the Cape or crossing a cold northern coast it drops to single figures, and the moisture that was in the air condenses on the steel and on the cartons.
Timber follows the air. The reason the packing target is 8–10% at packing rather than "as dry as possible" is that a container crossing the tropics can push 8% timber to 13% and back; starting at 8–10% leaves room for the round trip.
Carton board, not chairs. Cartons take on moisture and go soft, the print smears, and the stack loses its corner strength. On arrival the boxes look tired and the frames inside are fine — or the reverse, where the carton dried out and the chair picked up the moisture on the way through.
The second failure is at the bottom layer. Steel glides and powder-coated legs sit against damp carton board for a month. That is where you find rust bloom on a delivery that passed salt spray testing in the factory.
Desiccant. Two kilos of silica gel per pallet position, in perforated bags, checked against the loading plan. Not a cure, a buffer.
Liner. Vapour-barrier liner on the floor and lower walls keeps cartons off condensing steel. Costs about 40 dollars a container.
Loading position. Nothing against the doors. The door end of a container takes the worst of the condensation and the worst of the handling.
Open one carton per row on arrival and smell it. Damp carton has a distinct musty note. Then check the bottom layer of glides for bloom and the top layer of frames for surface checking — both are signs the box went through a cycle it was not packed for.